Chevy Hi-Performance Homepage
Prev Next
Adrian worked quickly, sliding the soaked pieces of fiberglass mat under the hood's metal ducting and into the repair area outlined by the metal mold. Note the brush, which helps position the mat and keep it wet with resin. Adrian built this area up until the proper thickness was achieved, which took 4-6 layers of 'glass mat.
Repairing Fiberglass Panels - Glass Act

Adrian worked quickly, sliding the soaked pieces of fiberglass mat under the hood's metal ducting and into the repair area outlined by the metal mold. Note the brush, which helps position the mat and keep it wet with resin. Adrian built this area up until the proper thickness was achieved, which took 4-6 layers of 'glass mat.  View Related Article